TEMPERATURE AND HEAT EFFECTS ON POLYETHYLENE BEHAVIOUR IN THE PRESENCE OF IMPERFECTIONS
ABSTRACT
This paper highlights the changes of polyethylene behaviour during various loading rate as well as the influence of test temperature on the material characteristics. Passive infrared thermography (IRT) method and a high speed infrared camera were used to observe the temperature changes of the sample surface during the tests. The experimental program was carried out on samples taken from PE80 polyethylene gas pipes with simulated imperfections with bilateral V-notch, U-notch and central hole. Samples have been tensile tested (TT) and the results are correlated with the temperature distribution of the samples surface.
KEYWORDS
PAPER SUBMITTED: 2015-11-10
PAPER REVISED: 2015-12-14
PAPER ACCEPTED: 2015-12-23
PUBLISHED ONLINE: 2016-01-01
THERMAL SCIENCE YEAR
2016, VOLUME
20, ISSUE
Issue 5, PAGES [1703 - 1712]
- Kratochvilla, T., Muschik, H., Dragaun, H., 2008. Experiences with modified test condition for notch pipe testing. J. Polym. Test. 27, pp. 158-160.
- Prabhakaran, R., Somasekharan, N., Sinha, E.M., 2003. Notch sensitivity of polymers. J. Appl. Polym. Sci. 22, pp. 3011-3020.
- Peres, F.M., Tarpani, J.R., Geraldo Schön, C.G., 2014. Essential Work of Fracture testing method applied to medium density polyethylene. Procedia Materials Science, 3, pp. 756 - 763.
- Linul, E., Voiconi, T., Marsavina, L. Determination of mixed mode fracture toughness of pur foams Structural Integrity and Life, Vol.14, No2, 2014, str. 87-92
- Pinter, G., Haager, M., Balika, W., Lang, R.W.,2007 Cyclic crack growth tests with CRB specimens for the evaluation of the long-term performance of PE pipe grades, J. Polym. Test. 26, pp. 180-188.
- Frank, A., Pinter, G., Lang, R.W., 2009. Prediction of the remaining lifetime of polyethylene pipes after up to 30 years in use, J. Polym. Test. 28, pp. 737-745.
- Murariu, A.C., Safta, V.I., Mateiu, H.S., 2010. Long-term behaviour of polyethylene PE 80 pressurized pipes, in presence of longitudinal simulated imperfections. Materiale Plastice, 47, pp. 263-266.
- Anderson, T.L., 2005. Fracture Mechanics. Fundamentals and Applications. Third Edition, CRC Press Inc.
- Uchida, M., Tada, N., Micro-, Meso- to Macroscopic Modeling of Deformation Behavior of Semi-Cystalline Polymer, 2013, Int. J. Plast. 49, pp. 164-184.